AISI Type 304HN Stainless Steel
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Heat Resisting; Metal
Close Analogs: AISI Type 304, 304L, 304HN
Key Words: aisi304, aisi 304, T304, T 304, SUS304, SS304, 304SS, 304 SS, T304HN, 304HN, 304 HN, UNS S30452, ASME S240 (XM-21), ASTM A240 (XM-21), ASTM A276 (XM-21), 18-8, high nitrogen
Material Notes: High Nitrogen 304 stainless steel. Austenitic Cr-Ni stainless steel. Nitrogen provides higher tensile and tensile yield strength without diminishing ductility, corrosion resistance, or nonmagnetic properties. Better corrosion resistance than Type 302. High ductility, excellent drawing, forming, and spinning properties. Essentially non-magnetic, becomes slightly magnetic when cold worked. Low carbon content means less carbide precipitation in the heat-affected zone during welding and a lower susceptibility to intergranular corrosion. Applications: Aircraft and Aerospace components, marine components, high temperature components, pressure vessels, pump components, welded tubing, forged fittings, pipe flanges, and valves. Weldability: Can be brazed and welded using common methods. Grain-boundary carbide precipitation can occur in heat-affected zones (HAZ). Annealing will restore corrosion resistance to the weldment.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 500°C
- Specific Heat Capacity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|