AISI Type 305 Stainless Steel, cold reduction 10%

 

Subcategory: Stainless Steel; T 300 Series Stainless Steel; Heat Resisting; Metal

Key Words: UNS S30500, AMS 5514, AMS 5685, AMS 5686, ASME SA193, ASME SA194, ASME SA240, ASTM A167, ASTM A240, ASTM A249, ASTM A276, ASTM A313, ASTM A314, ASTM A368, ASTM A473, ASTM A478, ASTM A492, ASTM A493, ASTM A511, ASTM A554, ASTM A580, FED QQ-S-763, FED QQ-W-423, SAE J405 (30305), DIN 1.4303, UNI X8 CrNi 19 10, JIS SUS 305, SUS 305 J1, AMS 5514, ISO 4954 X5CrNi1812E, ISO 683/13 13, 18-8

Material Notes:
Same corrosion resistance and Type 302, but much lower rate of work hardening. Excellent cold formability, good free spinning and cold heading properties, recommended for severe cold drawing. Applications include electronic parts and other drawn applications.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。