AISI Type 309S Stainless Steel, tested at 315°C (600°F)
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Heat Resisting; Metal
Close Analogs: AISI Type 309, AISI Type 309 S (Cb)
Key Words: UNS S30908, AMS 5523, AMS 5574, AMS 5650, ASME SA240, ASTM A167, ASTM A240, ASTM A276, ASTM A314, ASTM A473, ASTM A511, ASTM A554, ASTM A580, SAE J405 (30309S), DIN 1.4833, AFNOR Z 15 CN 24.13 (Fr), UNI X 6 CrNi 23 14, austenitic
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Izod Impact
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|