AISI Type 310 Stainless Steel, annealed sheet
  Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal 
Close Analogs: AISI Type 310S 
Key Words: UNS S31000, AISI 310, BS 1449 310S24, BS 970 310S31, DIN 1.4845, DIN X12CrNi23.21, ISO 2604-1 F68, JIS G4311 SUH310, JIS G4312 SUH310, JIS G4316 SUH310, ASME SA182 310, ASME SA213 310, ASME SA249, ASME SA312, ASME SA358, ASME SA403, ASME SA409, ASTM A167, ASTM A182, ASTM A213, ASTM A249, ASTM A276, ASTM A312, ASTM A314, ASTM A358, ASTM A403, ASTM A409, ASTM A473, ASTM A511, ASTM A554, ASTM A632, FED QQ-S-763, FED QQ-S-766, MIL SPEC MIL S-862, SAE J405 
Material Notes:  Austenitic chromium-nickel steel with high strength and excellent corrosion resistance.  Great for use in elevated temperature, sulfur-bearing gas environments. 
  
  
    | Available Properties | 
   
    
    - Density
 
- Hardness, Rockwell B
 
- Tensile Strength, Ultimate
 
- Tensile Strength, Yield
 
- Elongation at Break
 
- Modulus of Elasticity
 
- Izod Impact
 
- Electrical Resistivity
 
- Magnetic Permeability
 
- CTE, linear 20°C
 
- CTE, linear 250°C
 
- CTE, linear 500°C
 
- CTE, linear 1000°C
 
- Specific Heat Capacity
 
- Thermal Conductivity at Elevated Temperature
 
- Melting Point
 
- Solidus
 
- Liquidus
 
- Maximum Service Temperature, Air
 
 
   |   
   |   
 | 
   | 
  
  
    | Property Data | 
   
    
    This page displays only the text 
    of a material data sheet.
  
    To see MatWeb's complete data 
    sheet for this material (including 
    material property data, metal 
    compositions, material suppliers, 
    etc), please click the button below.  | 
   
    | 
    
     | 
    
   |   
 |   
  
   |