AISI Type 314 Stainless Steel, annealed sheet
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Material Notes: Has the highest heat-resisting properties of any chromium-nickel steel. Used when maximum resistance to carburization is desired.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
|
|
|
|