AISI Type 317 Stainless Steel, annealed plate
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Key Words: UNS S31700, AISI 317, DIN 1.4449, DIN X5CrNiMo1713, ASME SA240, ASME SA249, ASME SA312, ASME SA403, ASME SA409, ASTM A167, ASTM A240, ASTM A249, ASTM A269, ASTM A276, ASTM A312, ASTM A314, ASTM A403, ASTM A409, ASTM A473, ASTM A478, ASTM A511, ASTM A554, ASTM A580, ASTM A632, FED QQ-S-763, SAE J405
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|