AISI Type 321 Stainless Steel, annealed and cold drawn bar, 25 mm diam.
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Material Notes: Similar to Type 304 except Ti content helps prevent chromium carbide precipitation resulting from welding or elevated temperatures. Stabilized at annealing temperatures between 950-1010°C (1750-1850°F). Resists scaling and vibration fatigue. Applications include aircraft exhaust stacks and manifolds, chemical processing equipment, weld equipment, jet engine parts.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Charpy Impact
- Izod Impact
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|