AISI Type 329 Stainless Steel, annealed bar
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Heat Resisting; Metal
Key Words: UNS S32900, ASME SA268, ASTM A268, ASTM A511, SS 14 2324, SIS 14 2324, 453S
Material Notes: diameter of 25-75 mm
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Charpy Impact
- Electrical Resistivity
- CTE, linear 1000°C
- Specific Heat Capacity
- Melting Point
- Solidus
- Liquidus
|
|
|
|