AISI Type 403 Stainless Steel, soft tempered, wire 6.4 mm diameter
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Heat Resisting; Metal
Key Words: UNS S40300, AMS 5611, AMS 5612, ASTM A176, ASTM A276, ASTM A314, ASTM A473, ASTM A479, ASTM A511, ASTM A580, FED QQ-S-763, MIL SPEC MIL-S-863, B.S. En. 56 B, martensitic, SAE J405 (51403), DIN 1.4024, AFNOR Z 12 C 13 M, JIS SIS 403, B.S. 420 S 29, ISO 683/13 3
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Izod Impact
- Fatigue Strength
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|