AISI Type 405 Stainless Steel, tested at 540°C (1000°F)
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Heat Resisting; Metal
Key Words: UNS S40500, ASME SA240, ASME SA268, ASME SA479, ASTM A176, ASTM A240, ASTM A268, ASTM A276, ASTM A314, ASTM A473, ASTM A479, ASTM A511, ASTM A580, ferritic, FED QQ-S-763, MIL SPEC MIL-S-862, SAE J405 (51405), DIN 1.4002, AFNOR Z 6 CA 13 (France), UNI X 6 CrAl 13, JIS SUS 405, B.S. 405 S 17, ISO 683/13 2
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Izod Impact
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|