AISI Type 416Se Stainless Steel, tested at 260°C (500°F)
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal
Close Analogs: AISI Type 416
Key Words: UNS S41623, AMS 5610, ASME SA194, ASTM A194, ASTM A314, ASTM A473, ASTM A511, ASTM A581, ASTM A582, MIL SPEC MIL-S-862, SAE J405 (51416Se)
Material Notes: 25 mm diameter bar, oil quenched from 995°C, held at tempering temperature for 2 hours.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Izod Impact
- Shear Modulus
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|