AISI Type 420 Stainless Steel, tested at 315°C (600°F)
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Heat Resisting; Metal
Key Words: UNS S42000, AMS 5506, AMS 5621, ASTM A276, ASTM A314, ASTM A473, ASTM A580, FED QQ-S-763, FED QQ-S-766, FED QQ-W-423, MIL SPEC MIL-S-862, SAE J405 (51420), B.S. 420 S 37, B.S. CDS-18 (U.K), martensitic, DIN 1.4021, AFNOR Z 20 C 13 (Fr), UNI X 20 Cr 13, JIS SUS 420 J1, SS14 2303 (Sweden), ISO 683/13 4
Material Notes: 16.0 mm diameter bar, austenitized at 980°C for 30 minutes, oil quench, temper for 2 hours at 28°C above test temperature
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Charpy Impact
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|