AISI Type 430 Stainless Steel annealed at 815°C, tested at 540°C (1000°F)
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal
Close Analogs: Composition Notes: Iron content calculated as remainder.
Key Words: UNS S43000, AMS 5503, AMS 5627, ASME SA182, ASME SA240, ASME SA268, ASME SA479, ASTM A176, ASTM A182, ASTM A240, ASTM A268, ASTM A276, ASTM A314, ASTM A473, ASTM A479, ASTM A493, ASTM A511, ASTM A554, ASTM A580, ASTM A651, B.S. 430 S 15, ferritic, DIN 1.4016, AFNOR Z 8 C 17 (Fr), UNI X 8 Cr 17, JIS SUS 430, SS14 2320 (Sweden), FED QQ-S-763, FED QQ-S-766, FED STD-66, MIL SPEC MIL-S-862, SAE J405 (51430), ISO 683/13 8
Material Notes: One of the most widely used "non-hardenable" stainless steels; magnetic in all conditions, good physical and mechanical characteristics, about three-quarters the ductility of low carbon strip and inferior to chrome-nickel grades; cost less than chromium-nickel stainless steels. Applications: cabinet hardware, decorative appliance and automotive molding and trim, range hoods, restaurant equipment, drawn and formed parts and stampings. Corrosion Resistance: Excellent resistance to citric and nitric acid, sulfur gases; slightly less corrosion and heat resistant than Types 301, 302, and 304. Weldability: Poorer than Type 409; use common fusion and resistance techniques, but welds not suitable for rigorous service. Use AWS E/ER 308L or 430 weld filler. Processing: Annealed 430 is susceptible to stretcher strains and roping. Skin passing after annealing reduces the likelihood of stretcher strains, but can also reduce the ductility somewhat.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|