AISI Type 430F Stainless Steel tested at 760°C (1400°F)
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Heat Resisting; Metal
Close Analogs: AISI Type 430F(Se)
Key Words: UNS S43020, ASTM A314, ASTM A473, ASTM A581, ASTM A582, MIL SPEC MIL-S-862, SAE J405 (51430F), DIN 1.4104, AFNOR Z 10 CF 17 (Fr), UNI X 10 CRs 17, JIS SUS 430 F, SS14 2383 (Sweden), ferritic, ISO 683/13 8a
Material Notes: Molybdenum content optional. Annealed bar held at temperature for 1 hour and pulled at the rate of 1.3 mm per minute
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|