AISI Type 440B Stainless Steel
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal
Material Notes: Iron content above calculated as remainder. Higher hardness than Type 440A. Information provided by Chevron-Phillips Chemical Company, LLC.
| Available Properties |
- Density
- Modulus of Elasticity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |