AISI Type 446 Stainless Steel, Annealed Plate
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal
Key Words: ASME SA268; ASTM A176; ASTM A276; ASTM A314; ASTM A473; ASTM A511; ASTM A580, UNS S44600; FED QQ-S-763; FED QQ-S-766; Mil Spec MIL-S-862; SAE J405 (51466)
Material Notes: Iron content above calculated as remainder. The excellent corrosion resistance of this non-hardenable, ferritic stainless is due to the high chromium content. This allows use in applications such as heaters, burners, nozzles, electrodes, and metal-ceramic seals. Typical annealing temperatures are 730-815°C; followed by air or water quench.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell A
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|