AISI Type 660 Stainless Steel (A286) room temperature, cold drawn wire diameter of 4.45 mm, aged at 650°C (1200°F)
Subcategory: Stainless Steel; Heat Resisting; T 600 Series Stainless Steel; Metal
Key Words: UNS S66286 (UNS K66286), AMS 5525, AMS 5731, AMS 5732, AMS 5734, AMS 5735, AMS 5736, AMS 5737, AMS 5804, AMS 5805, ASME SA638, ASTM A453, ASTM A638, SAE J467 (A286); DIN 1.4980
Material Notes: Test specimens were cold drawn and aged for 16 hours at temperature given, wire diameter of 4.45 mm, reduced in area by 51% of original diameter.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|