AISI Type 661 Stainless Steel tested at -130°C (-200°F)
Subcategory: Stainless Steel; Heat Resisting; T 600 Series Stainless Steel; Metal
Key Words: UNS R30155, AMS 5376, AMS 5531, AMS 5532, AMS 5585, AMS 5768, AMS 5769, AMS 5794, AMS 5795, ANSI G81.40, ASTM A639, ASTM A567, DIN 1.4971
Material Notes: 16 mm diameter bar, heated to 1190°C for 1 hour, air cooled, heated to 730°C for 16 hours, air cooled.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Charpy Impact
- Machinability
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|