AISI Type S14800 Stainless Steel condition SRH950, tested at -73°C (-100°F)
Subcategory: Stainless Steel; T S10000 Series Stainless Steel; Precipitation Hardening Stainless; Metal
Key Words: UNS S14800, AMS 5601, AMS 5603; Precipitation Hardening
Material Notes: A precipitation-hardening stainless steel. Maintains high strength at elevated temperatures.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
|
|
|
|