AISI Type S14800 Stainless Steel condition SRH950, vacuum induction melted, tested at 24°C
Subcategory: Stainless Steel; T S10000 Series Stainless Steel; Precipitation Hardening Stainless; Metal
Key Words: UNS S14800, AMS 5601, AMS 5603; Precipitation Hardening
Material Notes: Specimens were vacuum induction melted, tested in transverse, 25 mm wide, 6.4 mm thick, with an edge notch-root radius of 0.018 mm.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Notched Tensile Strength
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
|
|
|
|