17-7 PH Stainless Steel, TH1050, bar and forgings
Subcategory: Stainless Steel; T S10000 Series Stainless Steel; Precipitation Hardening Stainless; Metal
Key Words: UNS S17700, double treatment alloy, TH1050, bar and forgings, 17-7PH, 17-7 PH, 17/7PH, 17/7 PH, Precipitation Hardening
Material Notes: Properties are measured in the longitudinal direction. Processing: TH1050 - heated to austenitic range, 1040°C (1900°F), and water quenched. Reheated to 760°C (1400°F) to precipitate carbides. Carbides cause the austenite transform to martensite after cooling below 15°C (60°F). Tempered at 565°C (1050°) Applications: high strength high temperature applications, chemical processing equipment, heat exchangers, power boilers, superheater tubes Corrosion Resistance: 17-7 PH is suitable for use in fresh water, industrial and marine atmospheres, and mild chemical and oxidizing environments. 17-7 PH should not be used in salt water or reducing environments.
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|