AISI Type S20910 Stainless Steel, 6.4 mm diameter rod, annealed at 1120°C, 45% cold reduction
Subcategory: Stainless Steel; T S20000 Series Stainless Steel; Heat Resisting; Metal
Key Words: UNS S20910, AMS 5764, AMS 5861, ASME SA182(XM-19), ASME SA240 (XM-19), ASME SA249 (XM-19), ASME SA312 (XM-19), ASME SA403(XM-19), ASME SA412 (XM-19), ASME SA479 (XM-19), ASTM A183 (XM-19), ASTM A240 (XM-19), ASTM A249 (XM-19), ASTM A269 (XM-19), ASTM A276 (XM-19), ASTM A312 (XM-19), ASTM A403 (XM-19), ASTM A412 (XM-19), ASTM A429 (XM-19), ASTM A479 (XM-19), ASTM A580 (XM-19)
Material Notes: Test specimen starting size of 6.4 mm diameter bar, annealed at 1120°C. Austenitic, corrosion resistant. Applications in the petroleum, chemical, pulp and paper, textile, food processing, and marine industries; combines good corrosion resistance and high strength. Components include pumps, valves and fittings, fasteners, cables, chains, screens and wire cloth, marine hardware, boat shafting, heat exchange parts, springs, and photographic equipment.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Machinability
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|