AISI Type S21900 Stainless Steel, 15% final cold reduction, stress relieving heat treatment 540°C (1000°F) for 2 hours, air cooled

 

Subcategory: Stainless Steel; T S20000 Series Stainless Steel; Heat Resisting; Metal

Close Analogs: AISI Type S21904

Key Words: UNS S21900, AMS 5561, ASTM A269 (XM-10), ASTM A276 (XM-10), ASTM A314 (XM-10), ASTM A412 (XM-10), ASTM A473 (XM-10), ASTM A580 (XM-10)

Material Notes:
Austenitic, high strength, excellent corrosion resistance, and low magnetic permeability. Applications include aircraft applications such as ducting and bellows systems, tail pipes and exhaust systems, clamps, fasteners, flanges, and hydraulic tubing. 10.2% relaxation, loss in load (starting condition: compression spring stress at 275 MPa at room temperature, exposed at 455°C for 5 days.)

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop
  • Hardness, Rockwell C
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Machinability
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。