AISI Type S24100 Stainless Steel 25 mm mill-annealed bar tested at 540°C (1000°F)

 

Subcategory: Stainless Steel; T S20000 Series Stainless Steel; Heat Resisting; Metal

Key Words: UNS S24100, ASTM A276 (XM-28), ASTM A313 (XM-28), ASTM A580 (XM-28)

Material Notes:
Low nickel, austenitic with comparable corrosion resistance, high work hardenability permits cold drawing to high-strength levels while maintaining good ductility, excellent wear- and galling-resistance, resists staining and rusting in 5% sodium chloride fog and high-humidity atmospheres, readily welded. Applications include high-strength shafting and bolting, clamps for pole line hardware, concrete reinforcing accessories, abrasion and corrosion resistant screens, high-strength nonmagnetic springs, wire forms, racks and cages.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Machinability
  • Electrical Resistivity
  • Magnetic Permeability
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。