AISI Type S30430 Stainless Steel soft tempered 2.54- 25.4 mm diameter wire
Subcategory: Stainless Steel; Heat Resisting; T S30000 Series Stainless Steel; Metal
Key Words: aisi304, aisi 304, UNS S30430, SUS304, SS304, ASTM A493 (XM-7), T S30430
Material Notes: Austenitic, exhibits lower rate of work than Type 305, non-magnetic in the annealed condition and becomes only very faintly magnetic after severe cold working, exhibits the same corrosion resistance as Type 304, subject to intergranular carbide precipitation when exposed to temperature ranges of 480-870°C, has a safe scaling temperature in continuous exposure of 870°C. Typical applications include cold formed nits and recessed head fasteners.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Modulus of Elasticity
- Shear Modulus
- Electrical Resistivity
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|