AISI Type S45000 Stainless Steel, 25 mm diameter bar, tested at -18°C (0°F), aged at 480°C (900°F)
Subcategory: Stainless Steel; Heat Resisting; T S40000 Series Stainless Steel; Metal
Key Words: UNS S45000, AMS 5763, ASME SA564 (XM-25), T S45000, ASME SA 705 (XM-25), ASTM A564 (XM-25), ASTM A693 (XM-25), ASTM A705 (XM-25)
Material Notes: Martensitic, age-hardenable, very good corrosion resistance with moderate strength, resists atmospheric corrosion including salt water atmospheres, excellent resistance to rusting and pitting in 5 and 20% salt spray at 35°C and oxidation up to 650°C, maximum service temperature for continuous service is 425°C. Niobium content minimum is 8 times the carbon content.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Notched Tensile Strength
- Charpy Impact
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|