AISI Type S45500 Stainless Steel, hardened at 540°C (1000°F) for 4 hours, air cooled, 1.3 mm round
Subcategory: Stainless Steel; Heat Resisting; T S40000 Series Stainless Steel; Metal
Key Words: UNS S45500, AMS 5578, AMS 5617, AMS 5672, AMS 5860, ASTM A313 (XM-16), ASTM A564 (XM-16), ASTM A705 (XM-16), marstensitic, T S45517
Material Notes: Martensitic, age-hardenable, easily formable (annealed), no corrosion in fresh water, resists staining in normal air atmosphere, good resistance to pitting in 5% salt spray and 5% ferric chloride. For use in service temperatures up to 425°C.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|