Ferralium Alloy 255 solution treated at 1120°C, cooled rapidly, 9.53 mm
Subcategory: Stainless Steel; Heat Resisting; Metal
Material Notes: Patented, ferritic-austenitic; high mechanical strength, ductility, and hardness with resistance to corrosion and erosion. Excellent resistance to acids and salts. Duplex alloy with nearly equal portions of austenite and ferrite-matrix phases. Applications include pumps, agitators, valves, and piping for handling wet phosphoric acid slurries, marine scrubbers, pumps and seals, and acid handling equipment.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|