ASTM A182, Grade F11, Class 1
Subcategory: Chrome-moly Steel; ASTM Steel; Low Carbon Steel; Metal
Close Analogs: ASME SA182 F11, UNS K11597
Key Words: ASME SA182 F11, UNS K11597, Cr-Mo alloys, chromium molybdenum alloys, chromoly steels, chro-moly
Material Notes: ASTM specifications tend to emphasize the performance aspects of specific end products rather than rigid chemical compositions. The specifications are often complete enough for procurement purposes. Better creep and environmental resistance than carbon steel. Applications: steam pipes, pressure vessels, turbine rotors, high temperature bolts Corrosion Resistance: offers relatively good corrosion resistance compared to cost Weldability easy to weld.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Specific Heat Capacity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|