ASTM A284 Steel, grade D
Subcategory: Carbon Steel; ASTM Steel; Low Carbon Steel; Metal
Key Words: AFNOR 35-501 E24-2, AFNOR 35-501 E24-3, BS4360 40(A)B, BS4360 40C, CSAG40-21230 G, DIN 17100 RSt 37-2, DIN 17100 St37-3U, EN10025(90) Fe E360B(FN), EN10025(90) Fe E 360 C, EN10025(93) S235JR(G2), EN10025(93) S235 J0, IS 226, IS Fe 410-S, JIS 3101 SS 400, JIS 3106 SM 400A, JIS 3106 SM 400B, ISO 630 Fe 360 B, ISO 630 Fe 360 C, MNC810E SS 13.11.00, MNC810E SS 13.12.00, NBN21-101 AE235B, NBN21-101 AE235 C, UNI 7070 Fe 360 B, UNI 7070 Fe 360 C
Material Notes: Carbon content increases with the thickness of the plate. Maximum thickness is 305 mm. Plates wider than 610 mm are tested in the transverse direction and the elongation requirement is reduced 2.0%
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bulk Modulus
- Shear Modulus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|