300M Ultrahigh Strength Steel
Subcategory: Carbon Steel; Low Alloy Steel; Medium Carbon Steel; Metal
Material Notes: Iron content calculated as balance. Phosphorous and sulfur content may vary. Silicon content helps to prevent embrittlement when tempered at low temperatures. Easily processed by hot forging; slow cooling is needed to prevent stress cracking.
| Available Properties |
- Density
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
|
|
|
|
| Property Data |