ASTM A573 Steel, grade 70
Subcategory: Carbon Steel; ASTM Steel; Low Carbon Steel; Metal
Close Analogs: ASTM A573 grade 50, grade 65
Key Words: UNS K02701
Material Notes: Intended for fusion welding and for service at atmospheric temperatures where improved notch toughness is important. Mn content is exceedable if C content plus Mn content is < 0.40%. The following are suggested consumables for arc welding processes: Manual Shielded Metal-Arc (AWS A5.5) Low Hydrogen Electrodes E7015, E7016, E7018, E7028; Submerged Arc (AWS A5.23) F7x-Exxx; Gas Metal-Arc (AWS A5.28) ER70S-x; Flux Cored-Arc (AWS A5.29) E7xT-x except -2, -3, -10, or -GS.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bulk Modulus
- Shear Modulus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|