ASTM A611 Steel, grade E
Subcategory: Carbon Steel; ASTM Steel; Low Carbon Steel; Metal
Close Analogs: ASTM A611 grade A, grade B, grade C, grade D
Key Words: copper steels, copper-steels
Material Notes: Cold rolled carbon steel sheet of structural quality in cut lengths or coils. Moderate ductility. Copper content of 0.20% is a minimum when copper steel is specified.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Bulk Modulus
- Shear Modulus
|
|
|
|