ASTM A678 Steel, grade C, plate thickness 19 - 38 mm
Subcategory: Carbon Steel; ASTM Steel; Low Carbon Steel; Metal
Close Analogs: ASTM A678 grade A, grade B
Key Words: UNS K02204
Material Notes: Copper content of 0.20% is a minimum when copper steel is specified. Maximum thickness is 50.8 mm. Plates wider than 610 mm were tested in the transverse direction and the elongation requirement was reduce by 2%. The following are suggested consumables for arc welding processes: Manual Shielded Metal-Arc (AWS A5.5) Low Hydrogen Electrodes E9015, E9016, and E9018; Submerged Arc (AWS A5.23) F9x-Exxx; Gas Metal-Arc (AWS A5.28) ER90S-x; Flux Cored-Arc (AWS A5.29) E9xT-x.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bulk Modulus
- Shear Modulus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|