ASTM A699 Steel, class 4
Subcategory: ASTM Steel; Low Alloy Steel; Low Carbon Steel; Metal
Close Analogs: ASTM A699 class 1, class 2, class 3
Key Words: UNS K10614
Material Notes: Precipitation heat treated 540 - 650°C (1200°F).
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bulk Modulus
- Shear Modulus
|
|
|
|
| Property Data |