ASTM A709 Steel, grade 36, carbon steel shapes (<= 634 kg/m)
Subcategory: ASTM Steel; Low Alloy Steel; Low Carbon Steel; Metal
Close Analogs: ASTM A709 grade 50
Material Notes: Maximum Mn content is 1.35% when notch toughness is specified. Not to be made from rimmed or capped steel.