ASTM A709 Steel, grade 50, high-strength, low alloy steel (<= 50 mm)
Subcategory: ASTM Steel; Low Alloy Steel; Low Carbon Steel; Metal
Close Analogs: ASTM A709 grade 36
Material Notes: Not to be made from rimmed or capped steel. Si content of 0.15 - 0.40% required for plates thicker than 38 mm. Mn to C ratio not to be less than 2:1.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bulk Modulus
- Shear Modulus
|
|
|
|