ASTM A633 HSLA Steel Grade D, Thickness 65 to 100 mm (2.5 to 4 in.)
Subcategory: ASTM Steel; Low Alloy Steel; Metal
Key Words: UNS K02003
Material Notes: Iron content calculated as balance. Manganese content spec depends on size and form. HSLA (High-strength low-alloy) steels are used for their higher strength and atmospheric corrosion resistance. They can be considered to be microalloyed steel and are designed for mechanical rather than compositional specs. ASTM A633 is used in welded, bolted, or riveted structures, above -45°C (-50°F) in which its strength and durability is required.
| Available Properties |
- Density
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
|
|
|
|
| Property Data |