ASTM A690 HSLA Steel, Thickness < 100 mm (4 in.)
Subcategory: ASTM Steel; Low Alloy Steel; Metal
Key Words: UNS K12249
Material Notes: Iron content calculated as balance. HSLA (High-strength low-alloy) steels are used for their higher strength and atmospheric corrosion resistance. They can be considered to be microalloyed steel and are designed for mechanical rather than compositional specs. ASTM A690 is noted for corrosion resistance in salt water splash zones so is used in docks, seawalls, bulkheads and related uses.
| Available Properties |
- Density
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Bend Radius, Minimum
|
|
|
|