ASTM A808 HSLA Steel, Thickness 50 - 65 mm (2 to 2.5 in.)
Subcategory: ASTM Steel; Low Alloy Steel; Metal
Material Notes: Iron content calculated as balance. HSLA (High-strength low-alloy) steels are used for their higher strength and atmospheric corrosion resistance. They can be considered to be microalloyed steel and are designed for mechanical rather than compositional specs. ASTM A808 is noted for good Charpy impact strength at low temperatures and is used in railway cars.
| Available Properties |
- Density
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Charpy Impact
- Shear Modulus
|
|
|
|