ASTM A841 HSLA Steel, Thickness 65 to 100 mm (2.5 to 4 in.)
Subcategory: ASTM Steel; Low Alloy Steel; Metal
Material Notes: Iron content calculated as balance. Manganese content may vary with thickness and carbon content. HSLA (High-strength low-alloy) steels are used for their higher strength and atmospheric corrosion resistance. They can be considered to be microalloyed steel and are designed for mechanical rather than compositional specs. ASTM 841 is used where its strength and durability is required such as welded pressure vessels.
| Available Properties |
- Density
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
|
|
|
|