ASTM A871 HSLA Steel Grade 65, Hot-Rolled, 5-20 mm (3/16 to 3/4 in.)
Subcategory: ASTM Steel; Low Alloy Steel; Metal
Material Notes: Iron content calculated as balance. HSLA (High-strength low-alloy) steels are used for their higher strength and atmospheric corrosion resistance. They can be considered to be microalloyed steel and are designed for mechanical rather than compositional specs. ASTM 871 is used where its strength and durability is required such as tubular structures and poles.
| Available Properties |
- Density
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
|
|
|
|
| Property Data |