AISI Type H12 Hot Work Tool Steel
Subcategory: Tool Steel; Hot Work Steel; Metal
Key Words: UNS T20812, ASTM A681, FED QQ-T-570, SAE J437, SAE J438, SAE J467, DIN 1.2606, UNI X 35 CrMoW 05 KU, JIS SKD 62, B.S. BH 12 (UK)
Material Notes: Oversized Charpy specimens austenitized at 1010°C for 1 hr., air-cooled, and double tempered to indicated hardness in Charpy Impact notes prior to grinding to finished size