HY-130 Steel
Subcategory: Carbon Steel; Low Alloy Steel; Low Carbon Steel; Metal
Key Words: HY130
Material Notes: Iron content calculated as balance. This quenched and tempered low-carbon alloy steel finds uses as pressure vessels, heavy construction equipment, and in large steel structures. It has high tensile strength (yield and ultimate), good ductility, notch toughness, atmospheric corrosion resistance, and weldability.
| Available Properties |
- Density
- Tensile Strength @ Yield
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
|
|
|
|