JIS S45C Steel, Tempered
Subcategory: Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel; Metal
Key Words: Similar to AISI 1045 and DIN CK45.
Material Notes: Very common grade in Asia.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Impact
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|