AISI Type S2 Tool Steel, austenitized 845°C (1550°F), brine quenched to 55 HRC
Subcategory: Tool Steel; Shock-Resisting Steel; Medium Alloy Steel; Metal
Close Analogs: AISI Type S1, AISI Type S4, AISI Type S5 AISI Type S6, AISI Type S7
Material Notes: Extremely strong and tough, recommended for applications where toughness is a top priority.
| Available Properties |
- Density
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bulk Modulus
- Shear Modulus
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
|
|
|
|