AISI Type A2 Tool Steel
Subcategory: Tool Steel; Air-Hardening Steel; Cold Work Steel; Metal
Key Words: AISI Medium-Alloy, Air-Hardening Tool Steels A2, UNS T30102, ASTM A681, FED QQ-T-570, SAE J437, SAE J438, DIN 1.2363, AFNOR Z 100 CDV 5 (Fr), JIS SKD 12, SS14 2260 (Sweden), B.S. BA 2
Material Notes: High hardenability, high degree of dimensional stability in heat treatment, good wear resistance, fatigue life, toughness, and deep hardening qualities. Applications include cold forming, blanking and bending dies, forming rolls, drill bushings, knurling tools, master dies and gages.
| Available Properties |
- Density
- Hardness, Rockwell C
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|