M50 Tool Steel
Subcategory: Tool Steel; High Carbon Steel; Metal
Material Notes: Excellent resistance to softening up to about 425°C (800°F). Good oxidation resistance and high compressive strength characteristic of high-speed tool steels. Applications: bearings and other parts for missiles aircraft engines; applications requiring high wear resistance and strength up to 425°C (800°F).