AISI Type W1 Tool Steel
Subcategory: Tool Steel; Water-Hardening Steel; High Carbon Steel; Metal
Material Notes: The highest quality, water hardening carbon tool steel, controlled for hardenability and subject to the most rigid tests to ensure maximum uniformity in performance, with a composition held to closest limits.
| Available Properties |
- Density
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
|
|
|
|
| Property Data |