Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si), Aged
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Near Alpha Titanium Alloy
Close Analogs: 1 other heat treatment of this alloy is in Matweb.
Material Notes: Sample Annealed 705ºC then aged 595ºC. Applications: High-temp jet engines. Blades, discs, spacers, seals. High performance automotive valves.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Beta Transus
|
|
|
|